Technical information:
Casted porcelain combined with hand modeling. Due to technological issues every cup undergo through four firings:
I. biscuit firing on 950C°
II. glazing + measures against deformation, firing on 1260C°
III. finishing of glazing and firing on 1220C°
IV. gold labels SEIN and firing on 750 C°